Impact of Deposits and Their Morphology on the Active Corrosion of Iron in Chlorine- and Sulfur-Containing Atmospheres in the Temperature Range of 350-500 °C
L. Krumm, M.C. Galetz
Oxidation of Metals 90 (2018), 365-381, DOI: 10.1007/s11085-018-9845-6